The following points should be noted when cutting wood grain film
The following points should be noted when cutting wood grain film
Wood grain film can be cut by wood grain film slitter
The following points should be noted when it is cut
1.Room Temperature Requirements:
The minimum process temperature is 18°C. The higher the temperature, the better the effect.
When the weather is cold, the film should be placed in the high temperature environment for 24 hours in advance.
The longer the storage time is, the better the cut effect will be.
2.The cutting blade must be replaced regularly
Otherwise, the flatness of the edge of the film after cutting can not be guaranteed.
Generally, the blade must be replaced after cutting the 5-6 film.
When the temperature is high in the summer, the using time can be increased.
3.Because the texture of the coating is relatively brittle, the cutting speed should not be too fast to prevent the cutting edge from being smashed.
In addition, the PVC powder on the edge of the film is too much.
Cutting too fast can easily cause the PVC powder to collect at the bottom of the plastic box.
It is easy to cause uneven gel distribution.
4.When the film is cut, the tolerance is controlled within ±0.5mm to avoid the small size.
If the size is too large, the tool can be used for trimming.
5.When the film is cut, as far as possible, the entire roll film is cut at one time according to the required specifications,
So as to avoid the incompleteness of the roll film and affect the filming quality.
Comment * I want material
Dear Mr Devdas Farakte
Thank you for your kind comment
Do you want to get wood grain film here? The supplier information can be sent after we get your confirmation
Best regards
Brightstar Aluminum Machinery